Mitigating the amorphization of perovskite solar cells by using atomic layer deposition alumina

Energy Environ. Sci., 2025, Accepted ManuscriptDOI: 10.1039/D4EE05703A, Paper Open Access &nbsp This article is licensed under a Creative Commons Attribution 3.0 Unported Licence.Mayank Kedia, Chittaranjan Das, Malgorzata Kot, Yenal Yalcinkaya, Weiwei Zuo, Kenedy Tabah Tanko, Peter Matvija, Mikel Ezquer, Iñaki Cornago, Wolfram Hempel, Florian Kauffmann, Paul Plate, Monica Lira-Cantu, Stefan A.L. Weber, Michael SalibaAtomic layer deposition of aluminum oxide (ALD-Al2O3) layers has been extensively studied for stabilizing perovskite solar cells (PSCs) against environmental stressors, such as humidity and oxygen. In addition, the ALD-Al2O3...The content of this RSS Feed (c) The Royal Society of Chemistry

Mar 12, 2025 - 11:44
 0
Mitigating the amorphization of perovskite solar cells by using atomic layer deposition alumina
Energy Environ. Sci., 2025, Accepted Manuscript
DOI: 10.1039/D4EE05703A, Paper
Open Access Open Access
Creative Commons Licence  This article is licensed under a Creative Commons Attribution 3.0 Unported Licence.
Mayank Kedia, Chittaranjan Das, Malgorzata Kot, Yenal Yalcinkaya, Weiwei Zuo, Kenedy Tabah Tanko, Peter Matvija, Mikel Ezquer, Iñaki Cornago, Wolfram Hempel, Florian Kauffmann, Paul Plate, Monica Lira-Cantu, Stefan A.L. Weber, Michael Saliba
Atomic layer deposition of aluminum oxide (ALD-Al2O3) layers has been extensively studied for stabilizing perovskite solar cells (PSCs) against environmental stressors, such as humidity and oxygen. In addition, the ALD-Al2O3...