Energy Environ. Sci., 2025, 18,5250-5263DOI: 10.1039/D4EE05703A, Paper Open Access &nbsp This article is licensed under a Creative Commons Attribution 3.0 Unported Licence.Mayank Kedia, Chittaranjan Das, Malgorzata Kot, Yenal Yalcinkaya, Weiwei Zuo, Kenedy Tabah Tanko, Peter Matvija, Mikel Ezquer, Iñaki Cornago, Wolfram Hempel, Florian Kauffmann, Paul Plate, Monica Lira-Cantu, Stefan A.L. Weber, Michael SalibaSchematic depiction of spiro-OMeTAD degradation causing perovskite instability under pseudo-operating conditions and its prevention using an ultra-thin ALD layer of alumina.The content of this RSS Feed (c) The Royal Society of Chemistry

Jun 3, 2025 - 16:30
 0
Mitigating the amorphization of perovskite layers by using atomic layer deposition of alumina

Energy Environ. Sci., 2025, 18,5250-5263
DOI: 10.1039/D4EE05703A, Paper
Open Access Open Access
Creative Commons Licence  This article is licensed under a Creative Commons Attribution 3.0 Unported Licence.
Mayank Kedia, Chittaranjan Das, Malgorzata Kot, Yenal Yalcinkaya, Weiwei Zuo, Kenedy Tabah Tanko, Peter Matvija, Mikel Ezquer, Iñaki Cornago, Wolfram Hempel, Florian Kauffmann, Paul Plate, Monica Lira-Cantu, Stefan A.L. Weber, Michael Saliba
Schematic depiction of spiro-OMeTAD degradation causing perovskite instability under pseudo-operating conditions and its prevention using an ultra-thin ALD layer of alumina.